Send Inquiry
Pig Iron for SteelmakingPig Iron GOST 805-95 (DSTU 3133-95)Pig Iron Grade Si Mn,group P, not more S, not more
1 2 3 4 Class Categories
From Up to Up to Up to Up to Up to ? B C 1 2 3 4 5
P1 0,5 0,9 0,5 1,0 1,5 - 0,10 0,20 0,30 0,01 0,02 0,03 0,04 0,05
P2 - 0,5
PL1 0,9 1,2 0,3 0,5 0,9 0,9 0,08 0,12
PL2 0,5 0,9 1,5
Mass of pigs not more then 18 kg without overcompression.
Residue of slag is not allowed on surface.
Quantity of breakages (pices of mass not more 2 kg) for Steelmaking pig iron: not more 4%
Carbon rates for Steelmaking pig iron: from 4 to 4,5%.
Offer from Ukrainian and Russian manufacturers.
Waiting for your inquiries.