Pad printing operation silicone rubber instructions Pad printing silicone rubber is two-component silicone, part A is the liquid silicone rubber, part B is the catalyst. The usual mxing ratio for silicone rubber and catalyst is 100 : 2-3, eg. we take 100grams of liquid silicone rubber, then we add 2-3 grams catalyst, mix then evenly and pour it to your mold. Then after 2-4 hours, you will obtain a printing pad. SHENZHEN HONG YE JIE TECHonOLOGY CO; LTD. Building A, No.3, Hongling First Road, Liulian Shibi, Pingdi Street, Longgang, Shenzhen, Guangdong, China Zip: 518117