Model:DNVAH32,ABSAH32
Ah32 steel plate for shipbuiling&platform.The shipbuilding steel plate grade AH32 is the high tensile strength steel.Ah32 shipbuilding steel is theHullstructural steel, with its good toughness properties, higher strength, strong corrosion-resistance, the processing properties, and welding properties. ASTM A131 Ah32 steel plate can be used in the manufacture of the ship's hull structure whose weight is more than 10000 tons.
Ah32 steel plate Chemical Composition %
| | C | Si | Mn | P | S | Als | Ti | Cu | Cr | Ni | Mo |
| AH32 | 0.18 | 0.50 | 0.90-1.60 | 0.035 | 0.035 | 0.015 | 0.02 | 0.35 | 0.20 | 0.40 | 0.08 |
Note: Generally speaking CE will be ≤ 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.36% (thickness ≤ 50mm),≤0.38%( when the thickness >50-100). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.
Ah32 steel plate Mechanical Property
| | Rm | Re(MPa) min | A% min | Akv/J min | ||||||
| AH32 | 440-570 | 315 | 22 | E.T °C | Thickness (mm) | |||||
| 0 | ≤ 50 | >50-70 | >70-100 | |||||||
| L | C | L | C | L | C | |||||
| 31 | 22 | 38 | 26 | 46 | 31 | |||||
Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.
Ah32 steel plate Condition Of Delivery
| | Fine grains elements | category | The thickness of steel | |||||
| ≤ 12 | >12.5-20 | >20-25 | >25-35 | >35-50 | >50-100 | |||
| AH32 | Nb+V or V | Plate/ | A(50) | N(50),CR(50),TM(50) | N(50),CR(25),TM(50) | |||
| Profile steel | N(50),CR(50),TM(50),AR*(25) | - | ||||||
| Al or Al+Ti | Plate/ | A(50) | AR*(25) | - | ||||
| N(50),CR(50),TM(50) | N(50),CR(25),TM(50) | |||||||
| Profile steel | A(50) | N(50),CR(50),TM(50),AR*(25) | - | |||||
Note: 1. delivery condition: A =Any; N=Normalized; CR=Control Rolled; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society; CR*=Can be control rolled with the agreement of Classification Society.
2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.
Contrast in the different standard
| | TOCT 5521 | JIS G3106 | BS LR | GB712 |
| AH32 | A32 | SM490B | AH32 | A32 |